Article 1
1. Member States are hereby authorized to derogate from the obligations arising under Article 1 of High Authority recommendation No 1-64 to the extent necessary to suspend at the levels indicated the customs duties on the products set out below, within tariff quotas of the amounts indicated for the Member States concerned:
1.2.3.4.5 // // // // // // CCT heading No // Description // Member State // Quota (tonnes) // Duty (%) // // // // // // ex 73.15 A V b) 1 and ex 73.15 B V b) 1 // Special wire rod for the manufacture of valve springs: (a) Of high carbon steel, not further worked than hot-rolled, between 5,5 and 13 mm in diameter with the following characteristics: // Germany Benelux France // 590 850 880 // 0 0 0 // // - Carbon: 0,60 to 0,70 % // // // // // - Silicon: not more than 0,25 % // // // // // - Manganese: 0,50 to 0,90 % // // // // // - Sulphur: not more than 0,020 % // // // // // - Phosphorus: not more than 0,030 % // // // // // - Copper: not more than 0,060 % // // // // // (b) Of chrome-vanadium alloy steel, not further worked than hot-rolled, between 5,5 and 13 mm in diameter, with the following characteristics: // // // // // - Carbon: 0,60 to 0,70 % // // // // // - Silicon: 0,15 to 0,30 % // // // // // - Manganese: 0,60 to 0,90 % // // // // // - Sulphur: not more than 0,025 % // // // // // - Phosphorus: not more than 0,025 % // // // // // - Chromium: 0,50 to 0,80 % // // // // // - Vanadium: 0,10 to 0,25 % // // // // // (c) Of chrome-silicon alloy steel, not further worked than hot-rolled between 5,5 and 13 mm in diameter, with the following characteristics: // // // // // - Carbon: 0,50 to 0,60 % // // // // // - Silicon: 1,20 to 1,70 % // // // // // - Manganese: 0,40 to 0,80 % // // // // // - Sulphur: not more than 0,025 % // // // // // - Phosphorus: not more than 0,025 % // // // // // - Chromium: 0,50 to 0,80 % // // // // // // // //
2. The abovementioned products must, in addition, comply with the following physical specifications:
1. Decarburization
Depth of decarburization measured without defects:
- high carbon and chrome-vanadium wire rod: 0,05 mm maximum,
- chrome-silicon wire rod: 0,07 mm maximum.
2. Surface condition
Maximum depth of defects (tears, fissures or folds) measured perpendicular to the surface: 0,05 mm
3. Non-metallic inclusions
Examination to be carried out in accordance with the AFNOR standard (reference A 04/106) of July 1972 and with Stahl-Eisen-Blatt 1570/71.
Typical maximum value figure 1 from the surface to two-thirds of the radius.
Typical maximum value figure 2 beyond two-thirds of the radius to the core.
The values indicated are valid for any type of inclusion. Article 2
1. Member States accorded quotas under Article 1 shall ensure, in liaison with the Commission, that such quotas are apportioned among third countries on a non-discriminatory basis.
2. They shall take all necessary steps to preclude the possibility of iron and steel products imported under the said tariff being re-exported, in the unaltered state to other Member States.
3. Community provisions on the matter shall apply for the purpose of verifying that the products in question are used for the particular purpose prescribed.